GENEVA, April 20 -- APPLIED MATERIALS, INC. (3050 Bowers AvenueSanta Clara, California 95054) filed a patent application (PCT/US2025/047113) for "COMBINED THERMAL AND PLASMA ASSISTED ATOMIC LAYER DEPOSITION" on Sep 19, 2025. With publication no. WO/2026/080210, the details related to the patent application was published on Apr 16, 2026.