Japan, Aug. 26 -- JFE STEEL CORP has got intellectual property rights for 'STEEL SHEET WITH EXCELLENT RESISTANCE TO AMMONIA STRESS CORROSION CRACKING AND METHOD FOR PRODUCING THE SAME.' Other related details are as follows:
Application Number: JP,2024-197756
Category (FI): C21D8/02@B,C21D8/0247,C21D8/0221,C21D8/021,C22C38/60,C22C38/00,301@B,C22C38/06
Stage: Grant (IP right granted following substantive examination.)
Filing Date: Nov. 12, 2024
Publication Date: May 29, 2025
The original document can be viewed at: https://www.j-platpat.inpit.go.jp/p0100
Disclaimer: Curated by HT Syndication....