MUMBAI, India, Jan. 9 -- Intellectual Property India has published a patent application (202541132934 A) filed by Annai Mira College Of Engineering And Technology, Chennai, Tamil Nadu, on Dec. 29, 2025, for 'a fire and thermal runaway mitigation barrier for electric vehicle batteries using nickel-based superalloy.'
Inventor(s) include Dr. Kanmani G.
The application for the patent was published on Jan. 9, under issue no. 02/2026.
According to the abstract released by the Intellectual Property India: "A fire and thermal runaway mitigation barrier system (100) comprising a battery enclosure, a nickel-based superalloy outer shield (102), a thermal insulation layer (104), a fire-retardant inner coating layer (106), a structural mounting frame...