ALEXANDRIA, Va., Sept. 8 -- United States Patent no. 12,730,082, issued on Sept. 8, was assigned to VERIDIS TECHNOLOGIES B.V. (Eindhoven, Netherlands).

"Massive differential scanning calorimetry analysis method and apparatus" was invented by Nigel David Jan Visser (Amsterdam), Floris Jelle Anton Gerritsen (Amsterdam) and Jeroen Dennis Glansdorp (Hoofddorp, Netherlands).

According to the abstract* released by the U.S. Patent & Trademark Office: "A method and apparatus of differential scanning calorimetry comprises: during the heating and/or cooling determining at least one of a temperature and a temperature change of the sample and of the reference; controlling a heating and/or cooling power to the sample and/or the reference on the basis ...