ALEXANDRIA, Va., Sept. 17 -- United States Patent no. 12,415,236, issued on Sept. 16, was assigned to Fulian Yuzhan Precision Technology Co. Ltd (Shenzhen, China).

"Method, apparatus, and non-transitory computer readable medium for detecting welding defects of workpieces" was invented by Tsung-Ju Lin (New Taipei, Taiwan), Meng Wang (Shenzhen, China), Cheng-Lun Lee (New Taipei, Taiwan), Chen-Ting Wu (New Taipei, Taiwan) and Huang-Ming Tseng (New Taipei, Taiwan).

According to the abstract* released by the U.S. Patent & Trademark Office: "A method for detecting welding defects of workpieces includes obtaining a first image from an image capturing element; extracting welding information from the first image; transmitting the welding informati...