GENEVA, March 11 -- THE TRUSTEES OF THE UNIVERSITY OF PENNSYLVANIA (3600 Civic Center Boulevard9th FloorPhiladelphia, Pennsylvania 19104) filed a patent application (PCT/US2025/044214) for "BANDGAP ENGINEERED QUANTUM DOT HETEROSTRUCTURES WITH POST SYNTHESIS COLLOIDAL ATOMIC LAYER DEPOSITION" on Aug 29, 2025. With publication no. WO/2026/050660, the details related to the patent application was published on Mar 05, 2026.

Notably, the patent application was submitted under the International Patent Classification (IPC) system, which is managed by the World Intellectual Property Organization (WIPO).

Inventor(s): KAGAN, Cherie R. (22 Derwen RoadBala Cynwyd, Pennsylvania 19004), NG, Jonah Jiayi (1620 Candlelight DriveLas Cruces, New Mexico 8801...