GENEVA, May 10 -- SIEMENS ENERGY GLOBAL GMBH & CO. KG (Otto-Hahn-Ring 681739 Munchen) filed a patent application (PCT/EP2025/079176) for "NICKEL BASE SUPERALLOY WITH LOW SHRINKAGE AND A COMPONENT" on Oct 09, 2025. With publication no. WO/2026/092984, the details related to the patent application was published on May 07, 2026.

Notably, the patent application was submitted under the International Patent Classification (IPC) system, which is managed by the World Intellectual Property Organization (WIPO).

Inventor(s): HASSELQVIST, Magnus (Torgvagen 1061213 Finspang)

Abstract: The invention relates to a Nickel based superalloy and a component of it comprising (in wt%) 12,0% to 15,0% Chromium (Cr), 1,0% to 2,0% Molybdenum (Mo), 3,0% to 12,0% T...