Japan, Jan. 16 -- JFE STEEL CORP has got intellectual property rights for 'THICK STEEL SHEET FOR WELDED STRUCTURE AND METHOD FOR MANUFACTURING THE SAME, METHOD FOR CREATING WELD DEFECT GENERATION PREDICTION MODEL, AND WELDED STRUCTURE.' Other related details are as follows:
Application Number: JP,2023-143441
Category (FI): C21D11/00,104,C21D8/021,C21D8/0221,C21D8/02@B,C22C38/00,301@B,C22C38/14,C22C38/58
Stage: Grant (IP right granted following substantive examination.)
Filing Date: Sept. 5, 2023
Publication Date: April 11, 2024
The original document can be viewed at: https://www.j-platpat.inpit.go.jp/p0100