MUMBAI, India, July 13 -- Intellectual Property India has published a patent application (202541000988 A) filed by Jeyavishnu K on January 05, 2025, for Pitting Corrosion Reagent Spray For Quantifying Metal Ions And Corrosion-Causing Agents.

Inventors include Jeyavishnu K; and Manish Malhan.

The application for the patent was published on July 10, 2026, under issue no. 28/2026.

Abstract: ABSTRACT Pitting Corrosion Reagent Spray for Quantifying Metal Ions and Corrosion-Causing Agents The present invention provides a method for detecting pitting corrosion on metal surfaces using a reagent solution [100] that contains chelating agents and color-forming compounds. This solution reacts with metal ions or corrosion agents, resulting in a color...